Project
Investigation of the role of alloying elements and hydrogen in the mechanical degradation of steam turbine steel due to stress-corrosion cracking in acidic water
Information
Project Team
Organisations
Outputs and Outcomes
Publications
An experimental investigation on the relation between corrosion and thermohydraulic behavior in heat exchangers for geothermal applications
Arne Simons
Willem Faes
Tom Depover
Steven Lecompte
Michel De Paepe
Kim Verbeken
A1
Journal Article
in
METALS
2024
The effect of coolant additives on the vapour explosion behaviour in melt droplet impingement experiments
Arne Simons
Inge Bellemans
Tijl Crivits
Kim Verbeken
A1
Journal Article
in
INTERNATIONAL JOURNAL OF HEAT AND MASS TRANSFER
2024
The influence of melt composition, liquidus temperature and solidus temperature on vapour explosions in melt droplet impingement experiments
Arne Simons
Inge Bellemans
Tijl Crivits
Kim Verbeken
A1
Journal Article
in
JOURNAL OF LOSS PREVENTION IN THE PROCESS INDUSTRIES
2023
The effect of an Al-induced ferritic microfilm on the hydrogen embrittlement mechanism in martensitic steels
Margot Pinson
Hauke Springer
Kim Verbeken
Tom Depover
A1
Journal Article
in
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING
2022
Stress corrosion cracking of steam turbine steel : the influence of organic acid characteristics
Tim De Seranno
Ellen Lambrechts
Arne Verliefde
Tom Depover
Kim Verbeken
A1
Journal Article
in
METALS
2022
The addition of aluminum to brittle martensitic steels in order to increase ductility by forming a grain boundary ferritic microfilm
Margot Pinson
Saurubh M. Das
Hauke Springer
Tom Depover
Kim Verbeken
A1
Journal Article
in
SCRIPTA MATERIALIA
2022
Investigation of the effect of carbon on the reversible hydrogen trapping behavior in lab-cast martensitic Fe-C steels
Margot Pinson
Lisa Claeys
H. Springer
Vitaliy Bliznuk
Tom Depover
Kim Verbeken
A1
Journal Article
in
MATERIALS CHARACTERIZATION
2022
The potential of the internal friction technique to evaluate the role of vacancies and dislocations in the hydrogen embrittlement of steels
Liese Vandewalle
Milan J. Konstantinović
Tom Depover
Kim Verbeken
A1
Journal Article
in
STEEL RESEARCH INTERNATIONAL
2021