Atomic layer deposition of composite Li-ion electrolytes for 3D thin film solid state batteries

Duration
01 January 2016 → 29 June 2019
Funding
Research Foundation - Flanders (FWO)
Research disciplines
  • Natural sciences
    • Condensed matter physics and nanophysics
    • Analytical chemistry
    • Physical chemistry
Keywords
MLD Energystorage Li-ion interface conductance composite solid elektrolyte ALD
 
Project description

The critical layer in a solid state battery is the electrolyte, which must be deposited conformally and with good thickness controll. To this end, lithiumsalts deposited with ALD or spincoating, will fill a porous inorganic matrix to form a solid electrolyte which improves the conductance orders of magnitude. Afterwards, these functional layers will be tested in 2D and 3D demonstrators.